Optical constants of SCHOTT - IRG
IRG 24
Wavelength:
µm
(0.8 – 15.5)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=2.8965+\frac{2.9567λ^2}{λ^2-0.1620}+\frac{0.9461λ^2}{λ^2-1939.1}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 1.80e-05 0 0 2.10e-07 0 1.67e-03 density: 4.41 g/cm3 thermal_expansion: - temperature_range: 20 100 ℃ coefficient: 20.0e-06 K-1 specific_heat: 0.37 J/(g·K) thermal_conductivity: - value: 0.18 W/(m·K) transition_temperature: 225 ℃ Knoop_hardness: 1.12 GPa fracture_toughness: 0.347 MPa·m1/2 shear_modulus: 8.5 GPa Youngs_modulus: 20.5 GPa
References
SCHOTT Infrared Chalcogenide Glasses - IRG 24 Product flyer (Version April 2017)
Data
INFO
Infrared glass
Often, calcogenide glasses are used in the optical systems operating at infrared wavelengths ~1-14 µm (for instance, optical systems for thermal imaging and night vision)Infrared glass types/brands from different makers
- AMTIR (an acronym for "Amorphous Material Transmitting Infrared Radiation"): Amorphous Materials Inc. (AMI)
- IG: VITRON
- IRG: SCHOTT
- BD: LightPath
- OPTIR: Rochester Precision Optics (RPO)
Cross-reference
Composition | AMI | VITRON | SCHOTT | LightPath | RPO |
---|---|---|---|---|---|
Ge33As12Se55 | AMTIR-1 | IG 2 | IRG 22 | OPTIR-1* | |
Ge30Sb13Se32Te25 | IG 3 | IRG 23* | |||
Ge10As40Se50 | IG 4 | IRG 24 | |||
Ge28Sb12Se60 | AMTIR-3* | IG 5 | IRG 25 | BD-2 | OPTIR-3* |
As40Se60 | AMTIR-2 | IG 6 | IRG 26 | BD6 | |
As40S60 | AMTIR-6 | IRG 27 |
External Links
- Infrared - Wikipedia
- Chalcogenide glass - Wikipedia
- AMTIR amorphous material transmitting IR radiation - Amorphous Materials
- Brief introduction: chalcogenide glasses - VITRON
- Infrared Chalcogenide Glasses - SCHOTT
- Optical resources and technical information - LightPath