Optical constants of OHARA - TIM (Titanate, medium-index)
L-TIM28P
Wavelength:
µm
(0.350 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{1.53013396λ^2}{λ^2-0.0114236857}+\frac{0.24536228λ^2}{λ^2-0.0555101852}+\frac{1.78233031λ^2}{λ^2-179.0743}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -6.17e-06 5.7e-09 -3.8e-11 9.99e-07 1.21e-09 0.26 nd: 1.694529 Vd: 30.655992 glass_code: 689311 density: 2.88 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 1.01e-05 K-1 - temperature_range: 20 300 °C coefficient: 1.3e-05 K-1 dPgF: 0.0073 climatic_resistance: 1.0 acid_resistance: 1.0 phosphate_resistance: 1.0
Comments
Low Softening Temperature
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets