Optical constants of OHARA - TIH (Titanate, high-index)
TIH6
Wavelength:
µm
(0.334 – 2.325)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.1200483-0.012774901λ^{2}+0.042416181λ^{-2}+0.0025526467λ^{-4}-0.00011907015λ^{-6}+2.3448425\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 ℃ nd: 1.805181 Vd: 25.432057 glass_code: 805254 glass_status: preferred
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets