Optical constants of OHARA - TIH (Titanate, high-index)
TIH23
Wavelength:
µm
(0.334 – 2.325)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.0578382-0.013332336λ^{2}+0.038204824λ^{-2}+0.0028735627λ^{-4}-0.00019421032λ^{-6}+2.6269529\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 ℃ nd: 1.784696 Vd: 26.298170 glass_code: 785263 glass_status: preferred
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets