Optical constants of OHARA - TIH (Titanate, high-index)
TIH14
Wavelength:
µm
(0.334 – 2.325)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.9828967-0.013103151λ^{2}+0.036731099λ^{-2}+0.0025467663λ^{-4}-0.00015569271λ^{-6}+2.3553872\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 ℃ nd: 1.761821 Vd: 26.517966 glass_code: 762265 glass_status: preferred
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets