Optical constants of OHARA - TIH (Titanate, high-index)
TIH11
Wavelength:
µm
(0.334 – 2.325)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.0547581-0.013301755λ^{2}+0.039295435λ^{-2}+0.0028224343λ^{-4}-0.00017708961λ^{-6}+2.6536608\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 ℃ nd: 1.784723 Vd: 25.677885 glass_code: 785257 glass_status: preferred
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets