Optical constants of OHARA - TIH (Titanate, high-index)
L-TIH53

Wavelength: µm
 (0.37 – 2.4)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=\frac{1.83464643λ^2}{λ^2-0.0134992001}+\frac{0.415079602λ^2}{λ^2-0.0618608854}+\frac{2.82563492λ^2}{λ^2-201.62917}$$

Conditions & Spec sheet

n_absolute: false
wavelength_vacuum: false
temperature: 25.0 ℃
thermal_dispersion:
  - type: "Schott formula"
    coefficients: -1.86e-06 8.76e-09 -1.88e-11 1.03e-06 1.4e-09 0.299
nd: 1.846660
Vd: 23.773536
glass_status: special
density: 3.34 g/cm3
thermal_expansion:
  - temperature_range: -30 70 ℃
    coefficient: 8e-06 K-1
dPgF: 0.0168
climatic_resistance: 3.0
acid_resistance: 1.0
phosphate_resistance: 1.0

Comments

Low Softening Temperature

References

OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

Ohara Group

Ohara Group is an international group of companies with headquarters in Japan and subsidiaries in Japan (Ohara, Inc.), United States (Ohara Corporation), and Germany (Ohara, GmbH). Ohara manufactures optical and electronic products and also offers measurement services, in particular measurement of refractive indices of solids and liquids.