Optical constants of OHARA - SSL
SSL2
Wavelength:
µm
(0.3 – 2.4)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.3006861-0.0098822575λ^{2}+0.013878959λ^{-2}+0.00016341277λ^{-4}+1.4393331\text{×}10^{-05}λ^{-6}-9.3322118\text{×}10^{-08}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 7.094e-06 0.0 0.0 0.0 0.0 0.0 nd: 1.529441 Vd: 51.722557 glass_code: 529517 glass_status: preferred density: 2.57 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 5.4e-06 K-1 - temperature_range: 20 300 °C coefficient: 6e-06 K-1 dPgF: -0.0067 acid_resistance: 1.0 phosphate_resistance: 1.0
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets