Optical constants of OHARA - PHM (Phosphate, medium-index)
PHM53
Wavelength:
µm
(0.334 – 2.325)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.5332354-0.0095005403λ^{2}+0.012923982λ^{-2}+0.00030691131λ^{-4}-1.7660009\text{×}10^{-05}λ^{-6}+1.0516051\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 ℃ nd: 1.603001 Vd: 65.479908 glass_code: 603655 glass_status: preferred
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)