Optical constants of OHARA - PBM (Plumbate, medium-index)
PBM3
Wavelength:
µm
(0.3 – 2.4)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{1.32567543λ^2}{λ^2-0.00973013804}+\frac{0.208112474λ^2}{λ^2-0.046285933}+\frac{1.15985207λ^2}{λ^2-137.559854}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 5.292e-06 0.0 0.0 0.0 0.0 0.0 nd: 1.612929 Vd: 36.994096 glass_code: 613370 glass_status: preferred density: 3.53 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 8.3e-06 K-1 - temperature_range: 20 300 °C coefficient: 9.5e-06 K-1 dPgF: -0.0001 acid_resistance: 1.0 phosphate_resistance: 2.0
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)