Optical constants of OHARA - PBL (Plumbate, low-index)
PBL25
Wavelength:
µm
(0.3 – 2.4)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.4465509-0.0097768464λ^{2}+0.01753112λ^{-2}+0.00095250889λ^{-4}-5.4837761\text{×}10^{-05}λ^{-6}+4.7303899\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 3.712e-06 0.0 0.0 0.0 0.0 0.0 nd: 1.581439 Vd: 40.753351 glass_code: 581408 glass_status: preferred density: 3.23 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 8.7e-06 K-1 - temperature_range: 20 300 °C coefficient: 9.8e-06 K-1 dPgF: -0.0005 acid_resistance: 1.0 phosphate_resistance: 2.0
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets