Optical constants of OHARA - PBL (Plumbate, low-index)
PBL1
Wavelength:
µm
(0.3 – 2.4)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.3489663-0.0075869873λ^{2}+0.016684762λ^{-2}+0.00017147637λ^{-4}+2.5194777\text{×}10^{-05}λ^{-6}+1.8523864\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 3.091e-06 0.0 0.0 0.0 0.0 0.0 nd: 1.548141 Vd: 45.781144 glass_code: 548458 glass_status: preferred density: 2.93 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 8.4e-06 K-1 - temperature_range: 20 300 °C coefficient: 9.7e-06 K-1 dPgF: -0.002 acid_resistance: 1.0 phosphate_resistance: 1.0
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets