Optical constants of OHARA - PBH (Plumbate, high-index)
PBH25W
Wavelength:
µm
(0.365 – 0.9)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.983028-0.01043595λ^{2}+0.03634647λ^{-2}+0.002619412λ^{-4}-0.0001751318λ^{-6}+2.13251\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 1.2821e-05 0.0 0.0 0.0 0.0 0.0 nd: 1.761797 Vd: 27.107726 glass_code: 762271 glass_status: preferred density: 4.79 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 7.5e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 8.5e-06 K-1 dPgF: 0.0085
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets