Optical constants of OHARA - PBH (Plumbate, high-index)
PBH23
Wavelength:
µm
(0.3 – 2.4)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.0554324-0.010867434λ^{2}+0.038522891λ^{-2}+0.0030173971λ^{-4}-0.0002129474λ^{-6}+2.4864803\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 1.457e-05 0.0 0.0 0.0 0.0 0.0 nd: 1.784702 Vd: 26.216753 glass_code: 785262 glass_status: preferred density: 4.99 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7.5e-06 K-1 - temperature_range: 20 300 °C coefficient: 8.7e-06 K-1 dPgF: 0.0092 acid_resistance: 3.2 phosphate_resistance: 3.0
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets