Optical constants of OHARA - PBH (Plumbate, high-index)
PBH13
Wavelength:
µm
(0.3 – 2.4)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.9161406-0.010147718λ^{2}+0.035077729λ^{-2}+0.0020869984λ^{-4}-0.00011077712λ^{-6}+1.7236453\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 1.094e-05 0.0 0.0 0.0 0.0 0.0 nd: 1.740769 Vd: 27.793228 glass_code: 741278 glass_status: preferred density: 4.44 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7.3e-06 K-1 - temperature_range: 20 300 °C coefficient: 8.4e-06 K-1 dPgF: 0.0097 acid_resistance: 1.2 phosphate_resistance: 2.0
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets