Optical constants of OHARA - PBH (Plumbate, high-index)
PBH1
Wavelength:
µm
(0.3 – 2.4)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{1.55408138λ^2}{λ^2-0.0120146818}+\frac{0.289397861λ^2}{λ^2-0.0532883208}+\frac{1.06727944λ^2}{λ^2-122.863029}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 1.076e-05 0.0 0.0 0.0 0.0 0.0 nd: 1.717362 Vd: 29.513538 glass_code: 717295 glass_status: preferred density: 4.47 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 8e-06 K-1 - temperature_range: 20 300 °C coefficient: 8.9e-06 K-1 dPgF: 0.0048 acid_resistance: 3.2 phosphate_resistance: 2.0
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets