Dispersion formula
$$n^2=2.266208-0.008895249λ^{2}+0.01260385λ^{-2}+0.0003758541λ^{-4}-1.385868\text{×}10^{-05}λ^{-6}+1.28332\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 8.9983e-07 0.0 0.0 0.0 0.0 0.0 nd: 1.517417 Vd: 52.412251 glass_code: 517524 glass_status: preferred density: 2.66 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 7.6e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 8.7e-06 K-1 dPgF: -0.002
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets