RefractiveIndex.INFO

Refractive index database


Shelf

Book

Page

Optical constants of OHARA - NBH (Niobate, high-index)
S-NBH57

Wavelength: µm
 (0.360 – 2.400)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=\frac{1.92026488λ^2}{λ^2-0.0118468028}+\frac{0.37153524λ^2}{λ^2-0.0532105472}+\frac{2.55205704λ^2}{λ^2-204.5493}$$

Conditions & Spec sheet

n_absolute: false
wavelength_vacuum: false
temperature: 25.0 ℃
thermal_dispersion:
  - type: "Schott formula"
    coefficients: -1.2e-06 8.85e-09 -1.11e-11 8.68e-07 1.05e-09 0.282
nd: 1.850249
Vd: 30.046429
density: 4.0 g/cm3
thermal_expansion:
  - temperature_range: -30 70 ℃
    coefficient: 7.7e-06 K-1
dPgF: 0.0051
climatic_resistance: 1.0
acid_resistance: 3.0
phosphate_resistance: 1.0

Comments

Recommended

References

OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

Ohara Group

Ohara Group is an international group of companies with headquarters in Japan and subsidiaries in Japan (Ohara, Inc.), United States (Ohara Corporation), and Germany (Ohara, GmbH). Ohara manufactures optical and electronic products and also offers measurement services, in particular measurement of refractive indices of solids and liquids.

External links


Glass

External links