Optical constants of OHARA - NBH (Niobate, high-index)
S-NBH53V
Wavelength:
µm
(0.330 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{1.65444141λ^2}{λ^2-0.0112485533}+\frac{0.267453927λ^2}{λ^2-0.052027274}+\frac{2.14530347λ^2}{λ^2-167.3661}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 3.11e-06 7.32e-09 -1.52e-11 8.38e-07 1.06e-09 0.264 nd: 1.737999 Vd: 32.326590 density: 3.19 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 7.1e-06 K-1 dPgF: 0.0008 climatic_resistance: 2.0 acid_resistance: 1.0 phosphate_resistance: 1.0
Comments
Recommended
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)