Optical constants of OHARA - LAM (Lanthanum, medium-index)
LAM61
Wavelength:
µm
(0.3 – 2.4)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{1.706024λ^2}{λ^2-0.009579771}+\frac{0.182716λ^2}{λ^2-0.04044097}+\frac{1.204833λ^2}{λ^2-127.571}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -1.7708e-06 0.0 0.0 0.0 0.0 0.0 nd: 1.720002 Vd: 46.035166 glass_code: 720460 glass_status: preferred density: 4.28 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 8.5e-06 K-1 - temperature_range: 20 300 °C coefficient: 9.6e-06 K-1 dPgF: -0.002 acid_resistance: 53.2 phosphate_resistance: 3.2
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets