Optical constants of OHARA - LAM (Lanthanum, medium-index)
LAM60
Wavelength:
µm
(0.334 – 2.325)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.9745038-0.014898498λ^{2}+0.022058854λ^{-2}+0.0007492073λ^{-4}-4.2104743\text{×}10^{-05}λ^{-6}+3.1048673\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 ℃ nd: 1.743198 Vd: 49.309053 glass_code: 743493 glass_status: preferred
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)