Optical constants of OHARA - LAM (Lanthanum, medium-index)
LAM52
Wavelength:
µm
(0.365 – 0.9)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.888081-0.01133043λ^{2}+0.02306135λ^{-2}+0.001004485λ^{-4}-5.630208\text{×}10^{-05}λ^{-6}+5.248466\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -8.8015e-07 0.0 0.0 0.0 0.0 0.0 nd: 1.720000 Vd: 43.705625 glass_code: 720437 glass_status: preferred density: 4.15 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 8e-06 K-1 - temperature_range: 20 300 °C coefficient: 9.1e-06 K-1 dPgF: -0.0008
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets