Optical constants of OHARA - LAM (Lanthanum, medium-index)
LAM51
Wavelength:
µm
(0.365 – 0.9)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.830675-0.01254193λ^{2}+0.01928173λ^{-2}+0.00113639λ^{-4}-8.838415\text{×}10^{-05}λ^{-6}+5.822869\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 4.8618e-06 0.0 0.0 0.0 0.0 0.0 nd: 1.699998 Vd: 48.078869 glass_code: 700481 glass_status: preferred density: 4.09 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 7.8e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 8.8e-06 K-1 dPgF: -0.0016
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets