Optical constants of OHARA - LAM (Lanthanum, medium-index)
LAM2
Wavelength:
µm
(0.334 – 2.325)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.967968-0.011312544λ^{2}+0.024812309λ^{-2}+0.00067776202λ^{-4}-1.0278339\text{×}10^{-05}λ^{-6}+2.1968703\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 °C nd: 1.743997 Vd: 44.787528 glass_code: 744448 glass_status: preferred
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets