Optical constants of OHARA - LAL (Lanthanum, low-index)
S-LAL52
Wavelength:
µm
(0.28 – 2.4)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.7418702-0.012719153λ^{2}+0.016306977λ^{-2}+0.00061414226λ^{-4}-4.8242632\text{×}10^{-05}λ^{-6}+2.8875864\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -4.1e-06 1.15e-08 3.8e-11 2.44e-07 2.82e-10 0.299 nd: 1.669999 Vd: 57.327972 glass_code: 670573 glass_status: special density: 3.96 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7.4e-06 K-1 - temperature_range: 20 300 °C coefficient: 8.9e-06 K-1 dPgF: -0.0049 climatic_resistance: 4.0 acid_resistance: 53.2 phosphate_resistance: 4.1
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)