Optical constants of OHARA - LAL (Lanthanum, low-index)
LAL8
Wavelength:
µm
(0.334 – 2.325)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.8795551-0.01462241λ^{2}+0.019128502λ^{-2}+0.00061342737λ^{-4}-3.5439045\text{×}10^{-05}λ^{-6}+2.1550362\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 °C nd: 1.712995 Vd: 53.845848 glass_code: 713538 glass_status: preferred
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets