Optical constants of OHARA - LAL (Lanthanum, low-index)
LAL61
Wavelength:
µm
(0.334 – 2.325)
Derived optical constants
n
k
logX
logY
eV
Dispersion formula
$$n^2=2.9706808-0.015058733λ^{2}+0.021490548λ^{-2}+0.00038566151λ^{-4}+4.1252602\text{×}10^{-06}λ^{-6}+1.0912892\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_is_absolute: false λ_is_vacuum: false temperature: 25.0 °C n_d: 1.740999 V_d: 52.648747 glass_code: 741527 glass_status: preferred
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets