Optical constants of OHARA - LAL (Lanthanum, low-index)
LAL60
Wavelength:
µm
(0.334 – 2.325)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.9223334-0.015268924λ^{2}+0.020070735λ^{-2}+0.00049690538λ^{-4}-1.5326299\text{×}10^{-05}λ^{-6}+1.0772354\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 °C nd: 1.725999 Vd: 53.565698 glass_code: 726536 glass_status: preferred
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)