Optical constants of OHARA - LAL (Lanthanum, low-index)
LAL13
Wavelength:
µm
(0.334 – 2.325)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.814252-0.013645728λ^{2}+0.018724991λ^{-2}+0.00056380326λ^{-4}-2.852714\text{×}10^{-05}λ^{-6}+1.8227195\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 ℃ nd: 1.693501 Vd: 53.231566 glass_code: 694532 glass_status: preferred
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets