Optical constants of OHARA - LAL (Lanthanum, low-index)
LAL12
Wavelength:
µm
(0.334 – 2.325)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.7589457-0.0087787656λ^{2}+0.021173055λ^{-2}-0.00047262367λ^{-4}+9.6870749\text{×}10^{-05}λ^{-6}-4.0576545\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 °C nd: 1.677900 Vd: 55.337587 glass_code: 678553 glass_status: preferred
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets