Optical constants of OHARA - LAL (Lanthanum, low-index)
L-LAL13
Wavelength:
µm
(0.28 – 2.4)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{1.17776146λ^2}{λ^2-0.00557618243}+\frac{0.634591345λ^2}{λ^2-0.0206821469}+\frac{1.20435649λ^2}{λ^2-99.6322776}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 1.27e-06 9.45e-09 -3.49e-11 5.82e-07 6.14e-10 0.192 nd: 1.693500 Vd: 53.185799 glass_code: 694532 density: 3.69 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7.6e-06 K-1 - temperature_range: 20 300 °C coefficient: 9.2e-06 K-1 dPgF: -0.0072 climatic_resistance: 2.0 acid_resistance: 53.2 phosphate_resistance: 4.0
Comments
Low Softening Temperature
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)