Optical constants of OHARA - LAH (Lanthanum, high-index)
S-LAH67
Wavelength:
µm
(0.3 – 2.4)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.1439609-0.015541721λ^{2}+0.026648169λ^{-2}+0.00077813143λ^{-4}-1.9462248\text{×}10^{-05}λ^{-6}+2.4668548\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 4.95e-06 0.0 0.0 0.0 0.0 0.0 nd: 1.794997 Vd: 45.293967 glass_code: 795453 glass_status: preferred density: 4.29 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 6e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 6.9e-06 K-1 dPgF: -0.0083 acid_resistance: 4.2 phosphate_resistance: 1.0
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets