Optical constants of OHARA - LAH (Lanthanum, high-index)
S-LAH65
Wavelength:
µm
(0.32 – 2.4)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{1.68191258λ^2}{λ^2-0.0077668425}+\frac{0.493779818λ^2}{λ^2-0.0288916181}+\frac{1.45682822λ^2}{λ^2-99.2574356}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 3.21e-06 1.28e-08 -3.45e-11 4.22e-07 5.14e-10 0.275 nd: 1.804000 Vd: 46.570373 glass_code: 804466 glass_status: preferred density: 4.76 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 6e-06 K-1 - temperature_range: 20 300 °C coefficient: 7.3e-06 K-1 dPgF: -0.009 acid_resistance: 4.1 phosphate_resistance: 1.0
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets