Optical constants of OHARA - LAH (Lanthanum, high-index)
LAH71
Wavelength:
µm
(0.3 – 2.4)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.3034137-0.013868754λ^{2}+0.037625274λ^{-2}+0.0021067685λ^{-4}-0.00011821055λ^{-6}+1.4781395\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 5.35e-06 0.0 0.0 0.0 0.0 0.0 nd: 1.850259 Vd: 32.285940 glass_code: 850323 glass_status: preferred density: 4.81 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7.4e-06 K-1 - temperature_range: 20 300 °C coefficient: 8.3e-06 K-1 dPgF: 0.0027 acid_resistance: 51.2 phosphate_resistance: 1.0
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets