Optical constants of OHARA - LAH (Lanthanum, high-index)
LAH67
Wavelength:
µm
(0.334 – 2.325)
Derived optical constants
n
k
logX
logY
eV
Dispersion formula
$$n^2=3.1439609-0.015541721λ^{2}+0.026648169λ^{-2}+0.00077813143λ^{-4}-1.9462248\text{×}10^{-05}λ^{-6}+2.4668548\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 °C nd: 1.794997 Vd: 45.293967 glass_code: 795453 glass_status: preferred
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets