Optical constants of OHARA - LAH (Lanthanum, high-index)
LAH65
Wavelength:
µm
(0.334 – 2.325)
Derived optical constants
n
k
logX
logY
eV
Dispersion formula
$$n^2=3.1767027-0.015350032λ^{2}+0.026690666λ^{-2}+0.00070784089λ^{-4}-1.5485093\text{×}10^{-05}λ^{-6}+1.9530666\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_is_absolute: false λ_is_vacuum: false temperature: 25.0 °C n_d: 1.804000 V_d: 46.575911 glass_code: 804466 glass_status: preferred
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets