Optical constants of OHARA - LAH (Lanthanum, high-index)
LAH63
Wavelength:
µm
(0.334 – 2.325)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.1647389-0.014742454λ^{2}+0.030279435λ^{-2}+0.0010475442λ^{-4}-2.4957393\text{×}10^{-05}λ^{-6}+4.4251949\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 °C nd: 1.804398 Vd: 39.581254 glass_code: 804396 glass_status: preferred
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets