Optical constants of OHARA - LAH (Lanthanum, high-index)
LAH59
Wavelength:
µm
(0.334 – 2.325)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.2178118-0.014296789λ^{2}+0.027199504λ^{-2}+0.00079036567λ^{-4}-2.3850632\text{×}10^{-05}λ^{-6}+2.0013066\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 ℃ nd: 1.816000 Vd: 46.626446 glass_code: 816466 glass_status: preferred
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets