Optical constants of OHARA - LAH (Lanthanum, high-index)
LAH51

Wavelength: µm
 (0.334 – 2.325)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula

$$n^2=3.110662-0.014462677λ^{2}+0.026457698λ^{-2}+0.00091877798λ^{-4}-3.3951573\text{×}10^{-05}λ^{-6}+3.325784\text{×}10^{-06}λ^{-8}$$

Conditions & Spec sheet

n_absolute: false
wavelength_vacuum: false
temperature: 25.0 ℃
nd: 1.785896
Vd: 44.186159
glass_code: 786442
glass_status: preferred

References

OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

Ohara Group

Ohara Group is an international group of companies with headquarters in Japan and subsidiaries in Japan (Ohara, Inc.), United States (Ohara Corporation), and Germany (Ohara, GmbH). Ohara manufactures optical and electronic products and also offers measurement services, in particular measurement of refractive indices of solids and liquids.