Optical constants of OHARA - LAH (Lanthanum, high-index)
L-LAH94
Wavelength:
µm
(0.350 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{2.0062142λ^2}{λ^2-0.0105499238}+\frac{0.347029888λ^2}{λ^2-0.0445845013}+\frac{1.41688382λ^2}{λ^2-105.99525}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 3.67e-06 9.08e-09 6.26e-13 4.07e-07 4.14e-10 0.194 nd: 1.860999 Vd: 37.097767 density: 4.89 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 6.2e-06 K-1 dPgF: -0.0029 climatic_resistance: 3.0 acid_resistance: 51.2 phosphate_resistance: 2.0
Comments
Low Softening Temperature
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)