Optical constants of OHARA - FTM
FTM8
Wavelength:
µm
(0.3 – 2.4)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.3063389-0.009299434λ^{2}+0.014148541λ^{-2}+0.00061944948λ^{-4}-3.542134\text{×}10^{-05}λ^{-6}+4.3560988\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -2.683e-06 0.0 0.0 0.0 0.0 0.0 nd: 1.532565 Vd: 45.914102 glass_code: 533459 glass_status: preferred density: 2.53 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 8.5e-06 K-1 - temperature_range: 20 300 °C coefficient: 9.7e-06 K-1 dPgF: 0.0077 acid_resistance: 1.0 phosphate_resistance: 1.0
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets