Optical constants of OHARA - FSL (Fluorosilicate, low-index)
S-FSL5Y
Wavelength:
µm
(0.28 – 2.4)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{0.977409944λ^2}{λ^2-0.00557649364}+\frac{0.210950834λ^2}{λ^2-0.0177000313}+\frac{1.37142848λ^2}{λ^2-149.211443}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -6.38e-06 1.6e-08 -3.75e-11 3.18e-07 4.69e-10 0.19 nd: 1.487490 Vd: 70.354425 glass_code: 487703 density: 2.46 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 8.9e-06 K-1 - temperature_range: 20 300 °C coefficient: 9.7e-06 K-1 dPgF: 0.0021 climatic_resistance: 2.0 acid_resistance: 3.0 phosphate_resistance: 2.0
Comments
Improved XMT at 365
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)