Optical constants of OHARA - BSM (Borosilicate, medium-index)
S-BSM21
Wavelength:
µm
(0.3 – 2.4)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{1.47867898λ^2}{λ^2-0.00869705653}+\frac{0.0899501399λ^2}{λ^2-0.0399353993}+\frac{1.03056525λ^2}{λ^2-108.550949}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 °C nd: 1.617195 Vd: 54.062144 glass_code: 617540 glass_status: preferred density: 3.49 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 6.5e-06 K-1 - temperature_range: 20 300 °C coefficient: 7.6e-06 K-1 dPgF: -0.0013 climatic_resistance: 2.0 acid_resistance: 1.0 phosphate_resistance: 1.0
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets