Optical constants of OHARA - BSM (Borosilicate, medium-index)
BSM16C
Wavelength:
µm
(0.3 – 2.4)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.5858505-0.011425977λ^{2}+0.013924703λ^{-2}+0.00050343054λ^{-4}-3.6074659\text{×}10^{-05}λ^{-6}+1.9912627\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 2.256e-06 0.0 0.0 0.0 0.0 0.0 nd: 1.620410 Vd: 60.254106 glass_code: 620603 glass_status: preferred density: 3.57 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 6.3e-06 K-1 - temperature_range: 20 300 °C coefficient: 7.4e-06 K-1 dPgF: -0.0014 acid_resistance: 52.2 phosphate_resistance: 3.2
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets