Optical constants of OHARA - BSM (Borosilicate, medium-index)
BSM15
Wavelength:
µm
(0.360 – 0.9)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.59025-0.009886858λ^{2}+0.01565646λ^{-2}+0.0002117553λ^{-4}+5.763945\text{×}10^{-06}λ^{-6}-3.134574\text{×}10^{-08}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 2.6586e-06 0.0 0.0 0.0 0.0 0.0 nd: 1.622992 Vd: 58.143312 glass_code: 623582 glass_status: preferred density: 3.65 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7e-06 K-1 - temperature_range: 20 300 °C coefficient: 8e-06 K-1 dPgF: -0.0017
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets