Optical constants of OHARA - BSL (Borosilicate, low-index)
L-BSL7
Wavelength:
µm
(0.3 – 2.4)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{0.917473918λ^2}{λ^2-0.00527701411}+\frac{0.352687665λ^2}{λ^2-0.0170809497}+\frac{1.05579788λ^2}{λ^2-104.302583}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 6.37e-06 1.48e-08 -4.17e-11 4.37e-07 7.14e-10 0.147 nd: 1.516330 Vd: 64.065129 glass_code: 516641 density: 2.38 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 5.8e-06 K-1 - temperature_range: 20 300 °C coefficient: 7.1e-06 K-1 dPgF: -0.0045 climatic_resistance: 3.0 acid_resistance: 1.0 phosphate_resistance: 1.2
Comments
Low Softening Temperature
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets
Data
INFO
BK7 optical glass
BK7 is a very popular crown glass. Most glass makers produce this glass under slightly different names.Analogs of BK7 glass produced by different makers
Maker | Glass |
---|---|
SCHOTT | N-BK7 |
OHARA | S-BSL7 |
HIKARI | J-BK7A |
CDGM | H-K9L |
HOYA | BSC7 |
SUMITA | K-BK7 |
LZOS | K8 |