Optical constants of OHARA - BSL (Borosilicate, low-index)
BSL22
Wavelength:
µm
(0.3 – 2.4)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.2739528-0.0091160058λ^{2}+0.01226882λ^{-2}-0.00031677862λ^{-4}+6.0075221\text{×}10^{-05}λ^{-6}-2.8098187\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 3.313e-06 0.0 0.0 0.0 0.0 0.0 nd: 1.518206 Vd: 65.039654 glass_code: 518650 glass_status: preferred density: 2.52 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 7.1e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 8.2e-06 K-1 dPgF: -0.0036 acid_resistance: 1.0 phosphate_resistance: 1.0
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets