Optical constants of OHARA - BSL (Borosilicate, low-index)
BSL21
Wavelength:
µm
(0.3 – 2.4)
Derived optical constants
n
k
logX
logY
eV
Dispersion formula
$$n^2=2.234734-0.0097856687λ^{2}+0.0098367633λ^{-2}+0.00021398416λ^{-4}-1.4554893\text{×}10^{-05}λ^{-6}+8.7393721\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 3.189e-06 0.0 0.0 0.0 0.0 0.0 nd: 1.503779 Vd: 66.814545 glass_code: 504668 glass_status: preferred density: 2.46 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 6.2e-06 K-1 - temperature_range: 20 300 °C coefficient: 7e-06 K-1 dPgF: -0.003 acid_resistance: 1.0 phosphate_resistance: 1.0
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets