Optical constants of OHARA - BPM (Borophosphate, medium-index)
BPM51
Wavelength:
µm
(0.3 – 2.4)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{1.37436455λ^2}{λ^2-0.00877165624}+\frac{0.174025602λ^2}{λ^2-0.0405249716}+\frac{0.905485504λ^2}{λ^2-72.7685343}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 7.297e-06 0.0 0.0 0.0 0.0 0.0 nd: 1.613397 Vd: 44.266767 glass_code: 613443 glass_status: preferred density: 3.24 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 5.2e-06 K-1 - temperature_range: 20 300 °C coefficient: 6.2e-06 K-1 dPgF: -0.0084 acid_resistance: 53.2 phosphate_resistance: 4.2
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets