Optical constants of OHARA - BPM (Borophosphate, medium-index)
BPM4
Wavelength:
µm
(0.3 – 2.4)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.5489492-0.012922911λ^{2}+0.018433588λ^{-2}+0.00067483064λ^{-4}-2.8837579\text{×}10^{-05}λ^{-6}+3.057603\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 7.898e-06 0.0 0.0 0.0 0.0 0.0 nd: 1.613400 Vd: 43.841533 glass_code: 613438 glass_status: preferred density: 3.22 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 5.3e-06 K-1 - temperature_range: 20 300 °C coefficient: 6.4e-06 K-1 dPgF: -0.008 acid_resistance: 53.2 phosphate_resistance: 4.2
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets